Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12 LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | ISO 178 |
Polyplastics Duranex® 407EP Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | ASTM D790 |
CPC - Vycom Corzan® CPVC Chlorinated PVC Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup.. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | JIS-K-6740 |
Denka VINYKON R3105 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Flexural Modulus | 2.49 GPa | 361 ksi | ASTM D-790 |
Axiall 7768 Rigid PVC, Extrusion Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen.. |