Polymer Property : Flexural Modulus = 2.448 GPa
Polymer Property :
Flexural Modulus =
2.448 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
2.448
GPa
355.1
ksi
ASTM D790
NYCOA 2025 Nylon 6
extrusion and molding grade with mold release and quicker cycle times for sports cleatsInformation provided by NYCOA, Inc.