Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ASTM D790 |
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East) LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ISO 178 |
Polyplastics Duranex® 200FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ISO 178 |
Polyplastics Duranex® 300FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ISO 178 |
Polyplastics Duranex® 500FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ISO 178 |
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ISO 178 |
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | ASTM D790 |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Flexural Modulus | 2.44 GPa | 354 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |