Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ISO 178 |
Radici Radilon® SHS (dry) Nylon 6 General PurposeInformation provided by Radici group. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM101R PC (Europe-Africa-Middle East) LEXAN FXM101R is a transparent/translucent high viscosity grade for special effects colors with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-IP .. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7687 PC (Europe-Africa-Middle East) ML7687 is an optical quality, high purity PC resin optimized for use in optical applications such as light guide panels |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | |
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 2.35 GPa @Thickness 6.40 mm |
341 ksi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000HU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.35 GPa @Thickness 3.20 mm |
341 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.35 GPa @Thickness 6.40 mm |
341 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Flexural Modulus | 2.35 GPa @Thickness 3.20 mm |
341 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2mm/min; ISO 178 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4736 is a PPO+HIPS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.This .. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX0888 PPE+PS Unfilled, non-FR. Higher heat resistance than N110 (BOZ) and px0844 (USA). For automotive interiors. 250F (121C) DTUL. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | |
Zylog Hipolyene® 3152 MC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 15mm/min; ASTM D790 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.6 mm/min; ASTM D790 |
BLUESTAR LXS 112 PPE-PS Typical Applications: PV Industrial partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 500H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |