Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000S PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5006B PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa | 328 ksi | ASTM D790 |
Hannam Chemical Hanalac H-2938 ABS |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Flexural Modulus | 2.26 GPa | 328 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Flexural Modulus | 2.26 GPa | 328 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | |
Shinil Chemical SHINCON ABS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0935 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 2.26 GPa | 328 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Flexural Modulus | 2.26 GPa | 328 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |