Polymer Property : Flexural Modulus = 2.243 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.243 GPa

@Thickness 19.0 mm
325.3 ksi

@Thickness 0.750 in
ASTM D790
3A Composites Core Materials AIREX® PXw.385 Fiber-Reinforced Structural Foam Panel
AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou..