Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.139 GPa | 310.2 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 1418 Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |