Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.07 GPa @Thickness 3.17 mm |
300 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer 7 MFR LEXAN HFD Copolymer |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Global PC-1418-IM Cold Temperature & Impact Modified Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | tangent; ASTM D790 |
Spartech PP5110 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 7000 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Statiblend® ABS AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Clariant Renol PA121 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Extrusion Grade Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness for all extrusion applications. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy