Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1340 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 19.0 GPa | 2750 ksi | ASTM D790 |
Greene Tweed Arlon® 1260 Polyketone, Carbon Filled Arlon® 1260 is a carbon-fiber reinforced version of Arlon 1000 featuring the highest modulus and tensile strength of all the Arlon grades. Designers requiring a low coefficient off thermal expan.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00DS PA 6 (Europe-Africa-Middle East) LNP THERMOCOMP* PF00DS is a compound based on PA6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Flexural Modulus | 19.0 GPa | 2750 ksi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6 LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA6.6 (Europe-Africa-Middle East) LNP Verton* RV00CESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | DIN 53 457 |
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton RV00CESP PA6.6 (Europe-Africa-Middle East) LNP* VERTON* RV00CESP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |