Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.45 GPa @Temperature 60.0 °C |
2531 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |