Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D-790 |
PlastiComp Complet® LCF15/LGF35 – PA66 BLK Polyamide 66, 50% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Flexural Modulus | 17.2 GPa @Temperature 23.9 °C |
2500 ksi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D790 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
(discontinued **) QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested.. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES HiFill® PA6 CF30 30% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 17.2 GPa | 2500 ksi | ASTM D790 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Flexural Modulus | 17.2 GPa | 2490 ksi | ASTM D790 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Flexural Modulus | 17.2 - 19.3 GPa | 2500 - 2800 ksi | Average value: 18.1 GPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |