Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.7 GPa @Thickness 3.20 mm |
2280 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID HM2604AW PA6+GF60% Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical |
|||
Flexural Modulus | 15.7 GPa | 2280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed) |
|||
Flexural Modulus | 15.7 GPa | 2280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 15.7 GPa | 2280 ksi | |
Phenolic 40%, Carbon fabric 60% Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1" |