Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.8 GPa | 2000 ksi | Lengthwise; ASTM D790 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific) LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | Lengthwise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 13.8 - 15.9 GPa | 2000 - 2300 ksi | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 |
PolyOne Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |