Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Flexural Modulus | 12.5 GPa @Temperature 23.0 °C |
1810 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DEL34E PC (Asia Pacific) LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
LATI LARPEEK 50 G/40 40% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Cookson Group Plaskon® SMT-B-1LV Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). Using an improved optimized filler system, it provide.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178-93 |
Wellman Wellamid® GF43-66 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
Unitika RUN35-TA Light resistant PA6, Conditioned Light resistant and internalInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | dry; ISO 178 |
DSM Stanyl® SC50 PA46-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
3M Filtek™ P60 Posterior Restorative Dental Composite Filtek P60 posterior restorative is an esthetic, light cured, radiopaque composite specifically designed for use in posterior direct or indirect restorations. Bonding to tooth structure is accompli.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 614 Nylon 6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)
(discontinued **) Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |