Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Plastcom SLOVAMID 66 GF 40 PA66, 40% glass fibre FeaturesChemically reinforced with 40% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | DIN 53 457 |
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead
(discontinued **) Improved Impact Strength, Low Flash, Low Warpage. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Hollow Articles Under Pressure, Pump HousingsProcessing: Injection Mo.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 80-7884 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | 2mm/min; ASTM D790 |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ASTM D790 |
IDI Composites M-203 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UX06028 PPA (Europe-Africa-Middle East) LNP * THERMOCOMP* UX06028 is a compund based on Polyphthalamide resin, containing Glass Fiber. Added features include Mold Release. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ISO 178 |
Polyplastics Freqtis® C0511A (PPS/LCP), Molding Compound Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In .. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ISO 178-93 |
Wellman Wellamid® WE1410 43% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | |
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa.. |
|||
Flexural Modulus | 12.0 - 16.0 GPa | 1740 - 2320 ksi | ISO 178 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |
|||
Flexural Modulus | 12.0 GPa | 1740 ksi | ISO 178 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |