Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.80 GPa | 1567 ksi | |
CMT Materials METAPOR® HD 210 AL Air Permeable Material METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi.. |
|||
Flexural Modulus | 10.80 GPa | 1567 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 GR15 WF25 Glass/Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |