Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.765 GPa | 256.0 ksi | ASTM D790 |
Tipco Tipcolene® FPC 10 - 10% Calcium Carbonate Reinforced Polypropylene Homopolymer 10% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Flexural Modulus | 1.765 GPa @Temperature 260 °C |
256.0 ksi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |