Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.69 GPa | 245 ksi | Tangent; ASTM D790 |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Flexural Modulus | 1.69 - 8.27 GPa | 245 - 1200 ksi | Average value: 3.45 GPa Grade Count:43 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5140H Compression Molding Polypropylene HomopolymerApplications: Compression Molded Caps and Closure ApplicationsFormolene 5140H DEVELOPMENTAL is a polypropylene homopolymer designed and formulated for compression molded caps and closure .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE) Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify i.. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | Chord, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1725 Performance Polyolefin Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior .. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 1.69 GPa | 245 ksi | ASTM D790 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |
|||
Flexural Modulus | 1.69 GPa @Temperature 23.0 °C |
245 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H07B-00 Polypropylene Homopolymer This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 17.. |