Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
PolyOne Trilliant™ HC THC-01-AS149031 Trans Blue Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Flexural Modulus | >= 1.62 GPa | >= 235 ksi | ASTM D790 |
S&E Specialty Polymers GPP1005M-EX8 PP Application: Polypropylene compound designed with halogen-based flame retardant technology meeting the UL 94 V-2 rating. Available in a wide range of colors and not subject to additive bloom.Info.. |
|||
Flexural Modulus | >= 1.62 GPa | >= 235 ksi | ASTM D790-79 |
S&E Specialty Polymers GPP™ 1005M-EX10 Natural PP Application: UL94 V-2, Non-blooming flame-retardant polypropylene compound for injection moldingInformation provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH005 Polypropylene, Homopolymer, Extrusion, Strapping COPYLENE® CH005 is a fractional melt flow polypropylene homopolymer resin available in pellet form.Information provided by Phillips 66. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
M. Holland Company PP410 Polypropylene Homopolymer AntistaticMedium flowGeneral purposeHomopolymerNucleatedApplications: Food containersGeneral purposeHousehold goodsToys |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
Hyosung Topilene HJ541CP PP HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G4K-038 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsma.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ISO 178 |
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 5 mm/min; ISO 178 |
Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 5 mm/min; ISO 178 |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.62 GPa @Temperature 23.0 °C |
235 ksi @Temperature 73.4 °F |
D790B |
Ineos N02J-00 Polypropylene Impact Copolymer This is a low melt flow rate, high impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact strength fo.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | secant; ASTM D790 |
Spartech PE4130 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
Samyang Trimma® SD6320 PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ISO 178-93 |
Wellman Wellamid® XT1816-BK1 Toughened Nylon 66 Description: Toughened Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6600 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AA60-003 Blow Molding Resin Product Description: AA60-003 is a medium molecular weight distribution high density polyethylene which is characterized by high stiffness, excellent melt uniformity, and chemical inertness.Availabi.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | ASTM D790 |
Ineos Nova 5490 High Impact Polystyrene
(discontinued **) High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an.. |
|||
Flexural Modulus | 1.62 GPa | 235 ksi | Tangent; ASTM D790 |
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products. |