Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.53 GPa | 222 ksi | ASTM D790 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | tangent; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | conditioned 15 days, 23°C - 50 % R.H.; ISO 178 |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® 4052F Polypropylene, Blown Film Grade Bapolene PP4052F is a PP homopolymer for blown film applications. It contains slip and antiblock additives as processing aids. It offers good clarity and optical properties. This product meets FD.. |
|||
Flexural Modulus | 1.53 GPa | 222 ksi | ASTM D790 |
Amco PRIMATOP HDPE RP 011 Granular High Density Polyethylene HDPE RP 011 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013. |