Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM040LN Polypropylene, Impact Copolymer, Thermoforming COPYLENE™ CM040LN is an impact copolymer specially designed for excellent processing in thermoforming applications and is formulated with antistat and nucleation. Applications: Thermoforming, Injec.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min, 1x3"; ASTM D790 |
Solvay Engineered Polymers DEXFLEX® 711-300 TPO
(discontinued **) Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color match.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR030LN Polypropylene, Mini-Random Copolymer, Thermoforming COPYLENE™ CR030LN is a mini-random copolymer with a high performance nucleation system designed to yield high clarity thermoformed articles.Applications: ThermoformingInformation provided by Philli.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | Tangent; ASTM D790 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | Tangent; ASTM D790 |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 5 mm/min; ISO 178 |
Gromax ATE90-FN01N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Spartech Formalloy LG Low-Gloss TPO Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | secant; ASTM D790 |
Spartech PP5220 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific) LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
CPC - Vycom SANATEC® Sanitary Cutting Boards High Density Polyethylene Sanatec is a high density polyethylene specially formulated for the manufacture of quality cutting boards. Sanatec`s special surface finish insures long product life and will not dull knives. Sanate.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | |
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy Anviloy® 1150 is a tungsten-based material that was developed primarily for die-casting, aluminum permanent mold, and difficult extrusions. It is produced by a high temperature powder metallurgy pr.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem D180A2 Homopolymer Polypropylene Description: Excellent Melt StabilityApplications: Suggested Uses Include Caps and Closures, Housewares, BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis re.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH008 Polypropylene, Homopolymer, Netting COPYLENE™ CH008 is a fractional melt flow polypropylene homopolymer resin available in pellet form. Applications: Raffia/Tapes/Strapping; Anti-Corrosion Coating; Geotextile & Agriculture; Nets. Rep.. |
|||
Flexural Modulus | 1.52 GPa | 220 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.52 - 24.0 GPa | 220 - 3480 ksi | Average value: 4.53 GPa Grade Count:124 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Flexural Modulus | 1.52 - 2.41 GPa | 220 - 350 ksi | Average value: 2.10 GPa Grade Count:10 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |