Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1405 TPO
(discontinued **) Description: SEQUEL® 1405 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, high flow and e.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total Finathene® SR 572 HDPE blow molding
(discontinued **) FINATHENE® SR 572 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® SR 572 has been developed for the manufacturing of blow molded bottles .. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol H007EG Polypropylene REPOL Polypropylene H007EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G2Z-026 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Low water carryover.Applications: Extrusion: tape and strapping.Former Huntsman polypropylene products are now produced by Flint Hills Resource.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Kuraray Genestarâ„¢ N1006A-M41 Nylon Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 65F5-2 Polypropylene Homopolymer, 20% Calcium Carbonate Key Features: conventional melt flow, medium high modulus, mineral-filled polypropylene homopolymer, high stiffness, excellent chemical resistance, good surface qualityApplications: automotive compo.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Iran Petrochemical (PCC) EPV 31 RA Polypropylene A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1100PK Polypropylene Homopolymer CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: MULTI - FILAMENT FOR BELTS, FIBRES FOR CARPETS INJECTION MOLDING FOR THIN WALL PARTS, HOUSEWARES |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strengthApplications: battery jars, electrical componentsDescription: Astryn BA905-74 med.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ TRA-3263EC/1 Thermoplastic Olefin Resin Key Features: fractional melt flow, high modulus, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good surface appearance, excellent processabilityApplicatio.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1mm/min; ISO 178 |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Borealis HD822CF Polypropylene HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total PPH 5069 Polypropylene Homopolymer, Fiber Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM-D790 |
Polyram PlusTek PB890 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM-D790 |
Polyram RamOfin PPC501 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | cond; ISO 178 |
DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0 20% Glass Reinforced, Flame Retardant, Halogen free |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | SAE J949 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Cathay PA512 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM Test |
BASF Styroclear GH 58 SBC Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 218 Polypropylene Homopolymer Applications include injection molding and fibers. Anti Gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |