Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM 5202 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D 790 |
Total Finathene® CD 522 HDPE corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790B |
Ineos 3950 Polypropylene Impact Copolymer Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Flexural Modulus | >= 1.31 GPa | >= 190 ksi | ASTM D790 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 50 mm/min span, 5 mm/min, 1 % secant; ASTM D790 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Flexural Modulus | >= 1.31 GPa | >= 190 ksi | ASTM D790 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 50 mm/min span, 5 mm/min, 1 % secant; ASTM D790 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D 790 |
Total PPC 4720 WZ Polypropylene, Impact Copolymer ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Ensinger Tecatron® XP-79 Compression Molded PPS Compound, 70% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow 5D98 Polypropylene Resin DOW 5D98 is intended for use in oriented polypropylene (OPP) film processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI41000WM Impact Copolymer Polypropylene Description: High flexural modulus, excellent mold release, antistatic.Applications: Suggested uses include intricately designed parts, thin-walled parts, dairy containers.Process: Injection Molding.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4700P2 Impact Copolymer Polypropylene Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thinwalled parts, dairy containers, building and const.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Asahi Kasei Thermofil P-10CC-1417 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D 790 |
Total PPC 4280W Polypropylene, Impact Copolymer ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hard.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790A |
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |