Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.255 GPa | 182.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin
(discontinued **) Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac.. |