Mechanical Properties Metric English Comments
Flexural Modulus 1.241 GPa
180.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Flex® TPO D-6500
Multi-Flex® D 6500 is well suited for TPO extrusion applications and certain high value molded parts for the telecommunications industry.Data provided by Multibase.
Flexural Modulus 1.241 GPa
180.0 ksi
Secant 1% strain; ASTM D-790-95
Multibase Multi-Pro® 0112 Black Polypropylene
Multi-Pro 0112 is a nucleated and antistated polypropylene homopolymer. It is designed for injection molding applications that require superior mold release properties.Data provided by Multibase.
Flexural Modulus 1.241 GPa
180.0 ksi
Tangent-Method 1; ASTM D790
Ineos B53-35H-011 HDPE
Ineos B53-35H-011 is a high density polyethylene copolymer developed for blow molding applications. This product is recommended for use in applications which require a combination of high top load ..
Flexural Modulus 1.241 GPa
180.0 ksi
Tangent-Method 1; ASTM D790
Ineos B53-35H-100 HDPE
B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica..
Flexural Modulus 1.241 GPa
180.0 ksi
Tangent; ASTM D 790
Ineos B54-25H-127 HDPE
B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Lucent Polymers CPP-0107 Polypropylene Homopolymer
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.241 GPa
180.0 ksi
Tangent; ASTM D 570
Ineos K54-05 HDPE
K54-05 is a high molecular weight, high density polyethylene copolymer developed for large-part blow molding (drum market) where the finished product demands outstanding physical performance. This m..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..