Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | tangent; ASTM D790 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 20-1202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-4IMP Impact Modified Nylon 66 for Injection Molding Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne |
|||
Flexural Modulus | 1.21 - 3.78 GPa | 175 - 548 ksi | Average value: 2.76 GPa Grade Count:9 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer COPYLENE® CM005 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes..Applications: Extrusion, sheet, film.Infor.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM350LN Polypropylene, Impact Copolymer, Medium Impact, Nucleated, Antistat, Injection Molding COPYLENE™ CM350LN is a high melt flow, controlled rheology, medium impact polypropylene copolymer resin designed for injection molding applications requiring a good balance of stiffness, impact, re.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP500 Polypropylene Copolymer Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive, Interior Parts Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformati.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 1% Tangent, 1.27 mm/min; ASTM D790 |
I. Stern 3335 Prime Impact Copolymer Polypropylene Features:Superior color and process stabilityLow odor, good flow and set up behaviorExcellent see through clarityApplicationsReusable food containersHousewaresPackagingInformation provided by I. Ste.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0901 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Blow MoldingExtrusionCoextrusionUses:TubingFurniturePipingInformation provided by Multibase |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 811 HS L (Dry) Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D709A |
Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AB50-003 Blow Molding Resin Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AF50-003 Blow Molding Resin AProduct Description: AF50-003 is a blow molding high density polyethylene copolymer containing an antistatic additive. It offers very good balance of stress crack resistance, stiffness and impact s.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | ASTM D790 |
Techmer ES Luriblend® HDPE GL5 Availability: North AmericaForms: PelletsAdditive: Graphite Powder LubricantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | >= 1.21 GPa | >= 175 ksi | tangent; ASTM D790 |
S&E Specialty Polymers GPP1001V0M-HCO PP Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flam.. |
|||
Flexural Modulus | 1.21 GPa | 175 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 350-10 RC Clarified Random Copolymer Features:excellent processingimpactclarityanti-statApplications:rigid packaginghousewaresFormer A-Top Polymers product; part of Amco product line since 2013. |