Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Flexural Modulus | 1.20 - 1.60 GPa | 174 - 232 ksi | ASTM D790-04 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Modulus | >= 1.20 GPa | >= 174 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1315M (YX37F) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 6329 Polypropylene Homopolymer, Improved Chemical Resistance Key Features: improved chemical resistance polypropylene homopolymer resin, FDA acceptable, easier processingApplications: closures, housewares, chairsMeets FDA requirements in 21 CFR 177.1520 for a.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer Key Features: blush-resistant, easy molding, high impact polypropylene copolymer resin, good cold impact resistance, good stiffness, FDA acceptableApplications: automotive battery case, housewares, .. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
MRC Polymers MAXTEL™ 650-BK Polypropylene Homopolymer • For injection molding• Excellent process ability with high flow.Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | Conditioned; ISO 178 |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO Method 178 |
LyondellBasell Astryn BA36GC Polypropylene Copolymer Key Features: conventional melt flow, medium modulus, UV-stabilized polypropylene copolymer, moderate stiffness, good impact resistance, low foggingApplications: seat valances, passenger assist hand.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ VB4411 TPO Compound Daplen VB4411 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen VB4411 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyplastics Duracon® TD-25 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM-D790 |
Braskem PRA 0852 RACO Random Polypropylene Copolymer PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processab.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 527-2 |
Total PPC 10712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
Ashley Polymers Ashlene® L935 Nylon 11 An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
Polyram RamOfin PPC104 Polypropylene Copolymer Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 1.20 - 3.38 GPa | 174 - 490 ksi | Average value: 2.60 GPa Grade Count:18 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Flexural Modulus | 1.20 GPa | 174 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000J5 is a compound based on PA 6 resin containing Impact Modifier.
Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |