Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/mm, 1% Secant; ASTM D790A |
Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mol.. |
|||
Flexural Modulus | 1.03 GPa @Thickness 3.20 mm |
150 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 301 Black 1284-11 S Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos TUB 121N HDPE TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GM 8250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Pro-faxâ„¢ SG722 Polypropylene Copolymer Description: Pro-faxâ„¢ SG722 high flow, high impact polypropylene copolymer resin is designed for injection molding applications. This resin is available in pellet form. Pro-faxâ„¢ SG722 res.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Spartech Royalstatâ„¢ R635 ABS/Polyolefin Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Sterigenics Raprex® R-100 Branched High Density Polyethylene Applications: ExtrusionRAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
ExxonMobil HDPE BU46-055 High Density Polyethylene Resin Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5021 Polypropylene, Blow Molding Grade Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product me.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3802 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA46-055 Blow Molding Resin Product Description: BA46-055 is a high molecular weight high density polyethylene copolymer. It possesses a combination of excellent processability, outstanding melt strength, high impact strength.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 - 3.10 GPa | 149 - 450 ksi | Average value: 1.89 GPa Grade Count:27 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |