Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.9770 GPa | 141.7 ksi | Secant @ 2%, 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |