Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.972 GPa | 141 ksi | Tangent; ASTM D790 |
Flint Hills P9R6K-054 Random Copolymer Polypropylene Excellent clarity. High flow material. Product does not contain any animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement for PET, .. |
|||
Flexural Modulus | 0.972 GPa | 141 ksi | Tangent; ASTM D790 |
Flint Hills P9R6K-054A Random Copolymer Polypropylene Features: Excellent clarity. High flow material. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement fo.. |