Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.931 GPa | 135 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
Multibase Multi-Pro® 3011 CHI Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | Tangent; ASTM D790 |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | >= 0.931 GPa | >= 135 ksi | ASTM D790-79 |
S&E Specialty Polymers GPP1001V0M-HCO-15 PP Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high lev.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 20-0202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790 |
Network Polymers NPP 25-0202 C Description: Copolymer Polypropylene, Clarified RandomInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 2% Secant; ASTM D 790 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | Procedure A; ASTM D790 |
M. Holland Company CP503 Polypropylene Impact Copolymer Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 1.33 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 150-1335 LMDPE Rotational Molding Resin Description: ICORENE 150-1335 is a linear medium density polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good proce.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 195-1336 LMDPE Rotational Molding Resin Description: ICORENE 195-1336 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive) Carbon-powder-filled, thermally stable, conductive material with consistent resistivities |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | ASTM D790 |
CPC - Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP) Flametec™ CP5 was formulated to meet the SEMI S93 specification for fire safety in clean room applications. CP5 meets UL 94 V-0 fire classification and is extruded for gauge and dimensional consist.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | |
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1 For arcing electrical contactsInformation provided by CMW Inc. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | |
CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Flexural Modulus | >= 0.931 GPa | >= 135 ksi | ASTM D790 |
Buckeye Polymers BP PPC 0210 R BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring increased impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resi.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 0.05 in/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 350-40 Polypropylene Copolymer PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6350WV High Impact Copolymer Polypropylene Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for.. |
|||
Flexural Modulus | 0.931 GPa | 135 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |