Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.896 GPa | 130 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-2001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790A |
Dow INSPIRE™ DT701-14 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman M3007-P Polyethylene
(discontinued **) M3007-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3007-P Has been found to exhibit good barrier properties, temperature resistance, and.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | Tangent; ASTM D790 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties) Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | secant; ASTM D790 |
Spartech PP7210 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790-90 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | |
Westlake MC2004 High Density Polyethylene Coating Westlake MC2004 is a high density polyethylene designed for extrusion coating and lamination applications. MC2004 provides improved barrier properties, temperature resistance, stress crack resistanc.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | ISO 178 |
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | |
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated For electrical contacts resistant to arcing and welding in circuit breakers, etc.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D790 |
ExxonMobil HD 8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D790 |
ExxonMobil HDP8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | Tangent; ASTM D790 |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.896 GPa @Temperature 175 °C |
130 ksi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Flexural Modulus | 0.896 - 2.30 GPa | 130 - 334 ksi | Average value: 1.52 GPa Grade Count:39 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D790 |
Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Da.. |