Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.895 GPa | 130 ksi | ASTM D790A |
Dow INSPIRE™ DT701-14 TPO
(discontinued **) High Flow, High Impact TPOInformation provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product l.. |