Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.858 GPa | 124 ksi | |
Kuraray SEPTON® PM1 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |