Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.855 GPa | 124 ksi | 2% Secant; Molded and tested per ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |