Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.853 GPa | 124 ksi | ASTM D760 |
LG Chemical SEETEC R3450 Polypropylene Random Copolymer Features: Seetec R3450 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |