Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.710 GPa | 103 ksi | ASTM D790 |
Huntsman Rexell® H2110 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: Good toughness, ESCR.Applications: Industrial and consumer pails, general purpose molding.Information provided by Huntsman Corporation |
|||
Flexural Modulus | 0.710 GPa | 103 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8660 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Flexural Modulus | 0.710 GPa | 103 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Flexural Modulus | 0.710 GPa | 103 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8660 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8660 is fully formula.. |
|||
Flexural Modulus | 0.710 GPa | 103 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formula.. |
|||
Flexural Modulus | 0.710 GPa | 103 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 826HS TPO
(discontinued **) Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and.. |