Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.558 GPa | 81.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.558 GPa | 80.9 ksi | ASTM D790 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Flexural Modulus | 0.558 GPa | 81.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Flexural Modulus | 0.558 GPa | 81.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Flexural Modulus | 0.558 GPa | 81.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene Compact™ RM8346RC Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346RC is a third generation linear medium density black polyethylene for rotational molding. Borecene RM8346RC is a special grade, which has passed rigorous tests and can be con.. |