Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.539 - 0.655 GPa | 78.2 - 95.0 ksi | Average value: 0.596 GPa Grade Count:10 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Flexural Modulus | 0.539 GPa | 78.2 ksi | ASTM D790 |
SK Chemicals SKYPEL G172D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Flexural Modulus | 0.539 - 0.637 GPa | 78.2 - 92.4 ksi | ASTM D790 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |