Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.448 GPa | 65.0 ksi | Tangent, 0.5 in/min; ASTM D790 |
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'.. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790(B) |
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp.. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
Ecomass® 4702ZB92 Filled Polyurethane Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
Ecomass® 4703ZB92 Filled Polyurethane Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers |
|||
Flexural Modulus | 0.448 GPa | 65.0 ksi | ASTM D790 |
DuPont™ Surlyn® PC350 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for proces.. |