Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.4275 GPa | 62.00 ksi | ASTM D790 |
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flexural Modulus | 0.4275 GPa | 62.00 ksi | 2% secant; ASTM D790 |
ExxonMobil LL 6100.17 Injection Molding Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |