Mechanical Properties Metric English Comments
Flexural Modulus 0.410 GPa
59.5 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE G 7680 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.410 GPa
59.5 ksi
ISO 178
Solvay Engineered Polymers DEXFLEX® E756 TPO  (discontinued **)
Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug..
Flexural Modulus 0.410 - 0.410 GPa

@Temperature 90.0 - 90.0 °C
59.5 - 59.5 ksi

@Temperature 194 - 194 °F
Average value: 0.410 GPa Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Flexural Modulus 0.410 GPa
59.5 ksi
ASTM D790
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Flexural Modulus 0.410 GPa
59.5 ksi
ASTM D790
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE.
Flexural Modulus 0.410 GPa
59.5 ksi
ASTM D790
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Flexural Modulus 0.410 GPa
59.5 ksi
ASTM D790
Chevron Phillips Marlex® 7104 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRGood melt strengthExcellent flexibilityGood processabilityGood glossHigh COFApplications: Landfill coversFlat and round-die productsCoext..