Mechanical Properties Metric English Comments
Flexural Modulus 0.356 GPa
51.6 ksi
3 pt. secant. ASTM D790
Chevron Phillips 7105T LLDPE Sheeting Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain..
Flexural Modulus 0.356 GPa
51.6 ksi
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex..