Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.284 GPa | 41.2 ksi | ISO 178 |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Flexural Modulus | 0.284 GPa | 41.2 ksi | ASTM D790 |
Toyobo PELPRENE™ S3002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |