Flexural Modulus | 0.2345 GPa | 34.01 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D 4508 D 4508 This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase. |