Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.234 GPa | 33.9 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 4502 BLK Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo.. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman D4027-P Voridian Polyethylene
(discontinued **) VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood Packa.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | ASTM D790 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 33.9 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Flexural Modulus | 0.234 - 45.0 GPa | 33.9 - 6530 ksi | Average value: 9.38 GPa Grade Count:74 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Flexural Modulus | 0.234 GPa | 34.0 ksi | Molded; ASTM D790 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |