Mechanical Properties Metric English Comments
Flexural Modulus 0.215 GPa
31.2 ksi
ISO 178
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Flexural Modulus 0.215 GPa
31.2 ksi
ASTM D790
Borealis Casico™ FR4802 Non-Halogen Flame Retardant Insulation/Jacketing Compound
Borstar FR4802 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4802 offers a unique combination of good extrusion p..
Flexural Modulus 0.215 GPa
31.2 ksi
ISO 178
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
Casico™ FR4820 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural insulation compound combining with excellent extrusion properties. It is based on the novel..