Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.168 GPa | 24.4 ksi | ASTM D790 |
DuPont 20 Series 20-6064 Specialty Polyethylene Resin DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding.. |