Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.103 GPa | 14.9 ksi | ASTM D790 |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 0.103 GPa | 14.9 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **) Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201.. |
|||
Flexural Modulus | 0.103 GPa | 14.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 812A Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not.. |
|||
Flexural Modulus | 0.103 GPa | 14.9 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 812P Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet... |
|||
Flexural Modulus | 0.103 - 19.3 GPa | 14.9 - 2800 ksi | Average value: 5.43 GPa Grade Count:176 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flexural Modulus | 0.103 GPa | 15.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 0.103 GPa | 15.0 ksi | 2% Secant; ASTM D790 |
Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Flexural Modulus | 0.103 GPa | 15.0 ksi | ASTM D790 |
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien.. |