Mechanical Properties Metric English Comments
Flexural Modulus 0.0965 GPa
14.0 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Flexural Modulus 0.0965 GPa
14.0 ksi
ASTM D790
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.0965 GPa
14.0 ksi
ASTM D790
Ecomass® 4703ZD84 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica..
Flexural Modulus 0.0965 GPa
14.0 ksi
2% Secant; ASTM D638
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional ..